This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2019, 10, 840–847, doi:10.3762/bjnano.10.84
Figure 1: Images of the experimental device for charging.
Figure 2: SEM and AFM images of a glass slide a) before and b) after the spray coating procedure.
Figure 3: Contact angle of water on the sprayed coating, before charging.
Figure 4: Changes in the contact angle as a function of voltage for the coating (T = 150 °C, t = 2 min).
Figure 5: Contact angle of the coating after charging for 2 min at 2000 V.
Figure 6: Contrast in wettability of the electrode contact area (after charging for 2 min at 2000 V) and the ...
Figure 7: SEM and AFM image of the electrode contact area (after charging for 2 min at 2000 V) in the coating....
Figure 8: Potential distribution of point 1: a) electrode non-contact area and b) electrode contact area.
Figure 9: Changes in the contact angle of the coating upon heating (2000 V, 2 min).
Figure 10: Changes in contact angle of the coating as a function of storage time for four charging times at 20...
Figure 11: Reversible conversion of coating superhydrophilicity–superhydrophobicity.
Figure 12: Durability of reversible conversion of coating superhydrophilicity–superhydrophobicity.